本文已被:浏览 2125次 下载 2070次
投稿时间:2017-02-13 修订日期:2017-02-28 录用日期:2017-02-28 网络发布日期:2017-05-19
投稿时间:2017-02-13 修订日期:2017-02-28 录用日期:2017-02-28 网络发布日期:2017-05-19
中文摘要: 某钴冶炼厂采用中和水解法除铁,在除铁过程中,存在除铁率低、铁渣中夹钴率高(达到14%)等问题。对此,采用中和水解法来降低除铜后钴浸出液中铁含量,对影响除铁的参数进行多因素试验。结果表明,在氧化还原电位0.40 V、终点pH在4.00~4.25、除铁时间控制在6.5 h以上、空气流量大于0.8倍溶液/min,除铁温度在50 ℃以上时,除铁率达到99%,钴夹带率降低到≤1%。
Abstract:A cobalt smelting plant applyies neutralizing hydrolysis process to remove iron. Process of iron removal has low iron removal rate and high cobalt entrainment in slag (up to 14%). Iron was removed from lixivium after copper removal by neutralizing hydrolysis process. Effect of parameter on iron removal was investigated. The results show that iron removal rate is 99% and cobalt entrainment rate is 1% below under the conditions including redox potential of 0.40 V, terminal pH value of 4.00~4.25, iron removal time of 6.5 h above, air flow of 0.8 time volum of solution per minute, and temperature of 50 ℃ above.
文章编号: 中图分类号: 文献标志码:
基金项目:无
| 作者 | 单位 | |
| 张素超* | 金川集团股份有限公司 镍钴研究设计院 | zhangsuchao@jnmc.com |
| 姚立学 | 金川集团股份有限公司 镍都实业公司 | |
| 卢苏君 | 金川集团股份有限公司 镍钴研究设计院 | |
| 张鹏 | 金川集团股份有限公司 镍钴研究设计院 |
| Author Name | Affiliation | |
| zhangsuchao | Jinchuan Group Co., Ltd. | zhangsuchao@jnmc.com |
| Yaolixue | ||
| Lusujun | ||
| Zhangpeng |
引用文本:
张素超,姚立学,卢苏君,张鹏.降低钴浸出液中铁杂质含量研究[J].有色金属(冶炼部分),2017(6):13-15.
zhangsuchao,Yaolixue,Lusujun,Zhangpeng.Study on Iron Removal from Cobalt Leaching Solution[J].Nonferrous Metals (Extractive Metallurgy),2017(6):13-15.
张素超,姚立学,卢苏君,张鹏.降低钴浸出液中铁杂质含量研究[J].有色金属(冶炼部分),2017(6):13-15.
zhangsuchao,Yaolixue,Lusujun,Zhangpeng.Study on Iron Removal from Cobalt Leaching Solution[J].Nonferrous Metals (Extractive Metallurgy),2017(6):13-15.