投稿时间:2014-05-11 修订日期:2014-05-13 录用日期:2014-05-16 网络发布日期:2014-10-15
中文摘要: 用甲酸为还原剂在硝酸体系中浸取低品位软锰矿,通过单因素试验和响应面法考察了甲酸用量、硝酸浓度、液固比、反应时间和反应温度对锰、铁、铝浸出率的影响。结果表明,当甲酸用量一定时,影响锰浸出率的因素主次依次是液固比、硝酸浓度、反应时间和反应温度。当甲酸用量为3 mL、硝酸浓度0.45 mol/L、液固比5.6、反应温度90 ℃、反应时间2.5 h时,锰、铁和铝的浸出率分别为91.01%、43.06%、21.61%。
Abstract:Pyrolusite was leached in nitric acid system with formic acid as reductant. The effects of dosage of formic acid, concentration of nitric acid, ratio of liquid to solid (L/S), reaction time, and reaction temperature on leaching rate of Mn, Fe, and Al by single-factor experiments and response surface methodology. The results show that the main influence factors on manganese leaching rate in sequence is L/S, concentration of nitric acid, leaching time and reaction temperature when dosage of formic acid is certain. The extraction rates of Mn, Fe, and Al is 91.01%, 43.06% and 21.61%, respectively under the optimum conditions including dosage of formic acid of 3 mL, nitric acid concentration of 0.45 mol/L, L/S of 5.6, leaching temperature of 90 ℃, and leaching time of 2.5 h.
文章编号: 中图分类号:TF803.2 文献标志码:
基金项目:2013广西高校锰深加工平台项目
| 作者 | 单位 | |
| 卢友志* | 广西民族大学化学化工学院 | luyzmail@163.com |
| 马少妹 | 广西民族大学化学化工学院 | 435109546@qq.com |
| 韦冬萍 | 广西民族大学化学化工学院 | dpwei-82@163.com |
| 袁爱群 | 广西民族大学化学化工学院 | aiqunyuan1999@sina.com |
| 黄宝英 | 广西民族大学化学化工学院 | 2030894680@qq.com |
引用文本:
卢友志,马少妹,韦冬萍,袁爱群,黄宝英.甲酸-硝酸还原浸出低品位软锰矿[J].有色金属(冶炼部分),2014(11):4-8.
LU You-zhi,MA Shao-mei,WEI Dong-ping,YUAN Ai-qun,HUANG Bao-ying.Reductive Leaching of Manganese from Low-grade Pyrolusite with Formic Acid in Nitric Acid System[J].Nonferrous Metals (Extractive Metallurgy),2014(11):4-8.
卢友志,马少妹,韦冬萍,袁爱群,黄宝英.甲酸-硝酸还原浸出低品位软锰矿[J].有色金属(冶炼部分),2014(11):4-8.
LU You-zhi,MA Shao-mei,WEI Dong-ping,YUAN Ai-qun,HUANG Bao-ying.Reductive Leaching of Manganese from Low-grade Pyrolusite with Formic Acid in Nitric Acid System[J].Nonferrous Metals (Extractive Metallurgy),2014(11):4-8.

关注微信公众号