本文已被:浏览 2591次 下载 2700次
投稿时间:2014-01-03 修订日期:2014-01-07 录用日期:2014-01-08 网络发布日期:2014-06-23
投稿时间:2014-01-03 修订日期:2014-01-07 录用日期:2014-01-08 网络发布日期:2014-06-23
中文摘要: 采用氧化焙烧脱硫、除碳—碳酸钠溶液浸出钼—浸钼渣氰化提金新工艺处理某金钼混合精矿。结果表明,在下述最佳试验条件下:粗精矿于600 ℃氧化焙烧1.5 h、钼焙砂加入矿重40%的碳酸钠后按液固比3~4在80~90 ℃浸出1.0~1.5 h,钼浸出率为91%,浸钼渣金的氰化浸出率大于95%。
Abstract:Low grade gold-molybdenum mixed concentrate was treated by new processes of desulfurization and decarbonization by oxidizing roasting, molybdenum leaching with sodium carbonate, and gold cyaniding from molybdenum leaching residue. The results show that molybdenum leaching rate is 91% when rough concentrate is oxidization roasted at 600 ℃ for 1.5 h, molybdenum calcining is leached at 80~90 ℃ for 1.0~1.5 h by sodium carbonate of 40% of weight of calcining with ratio of liquid to solid of 3~4. Gold cyaniding leaching rate from molybdenum leaching residue is 95% above.
keywords: gold-molybdenum mixed concentrates oxidizing roasting sodium carbonate leaching separation
文章编号: 中图分类号: 文献标志码:
基金项目:国土资源地质调查项目(1212011120305)
| 作者 | 单位 | |
| 曹耀华* | 中国地质科学院郑州矿产综合利用研究所 | cao2078@126.com |
| 李清 | 河南省工业学校 | |
| 高照国 | 中国地质科学院郑州矿产综合利用研究所 | zhaoguozzs@163.com |
| 刘红召 | 中国地质科学院郑州矿产综合利用研究所 | |
| 王威 | 中国地质科学院郑州矿产综合利用研究所 |
引用文本:
曹耀华,李清,高照国,刘红召,王威.低品位金钼混合精矿提取金钼新工艺[J].有色金属(冶炼部分),2014(7):42-44.
caoyaohua,liqing,gaozhaoguo,liuhongzhao,wangwei.New Process for Gold and Molybdenum Extraction from Low Grade Gold-Molybdenum Mixed Concentrate[J].Nonferrous Metals (Extractive Metallurgy),2014(7):42-44.
曹耀华,李清,高照国,刘红召,王威.低品位金钼混合精矿提取金钼新工艺[J].有色金属(冶炼部分),2014(7):42-44.
caoyaohua,liqing,gaozhaoguo,liuhongzhao,wangwei.New Process for Gold and Molybdenum Extraction from Low Grade Gold-Molybdenum Mixed Concentrate[J].Nonferrous Metals (Extractive Metallurgy),2014(7):42-44.