中文摘要: 以传统锌冶炼富含镓、锗的低酸浸出渣为原料,考察反应温度、时间、硫酸浓度等因素对镓、锗、锌、铁浸出率的影响。在综合试验条件下:反应温度95 ℃、初始酸度153 g/L、反应时间3 h、液固比5.9∶1,锌、铁、镓、锗浸出率分别达到88%、93%、88%、68%。浸出液经中和、锌精矿还原后可进一步富集回收镓、锗。
Abstract:The effects of reaction temperature, reaction time and sulfuric acidity on leaching rates of Ga, Ge, Zn and Fe were tested with the leaching residue containing gallium and germanium produced in traditional zinc metallurgical process as raw materials. The optimum comprehensive experiment conditions include reaction temperature of 95 ℃, initial acidity of 153 g/L, and reaction time of 3 h, L/S=5.9/1. Under the above conditions, the leaching ratio of zinc, iron, gallium, and germanium can reach 88%, 93%, 88%, 68% respectively. Ga and Ge can be concentrated from the leaching solution after neutralization and reduction.
keywords: Zinc metallurgy Leaching residue Gallium Germanium Leaching
文章编号: 中图分类号: 文献标志码:
基金项目:国家高技术研究发展计划(863计划)项目(2009AA064604)
| Author Name | Affiliation |
| WANG Yu-fang | Beijing General Research Institute of Mining and Metallurgy |
引用文本:
王玉芳.锌冶炼过程中镓锗的综合回收[J].有色金属(冶炼部分),2011(11):38-40.
WANG Yu-fang.Comprehensive Recovery of Ga & Ge in Zinc Metallurgy[J].Nonferrous Metals (Extractive Metallurgy),2011(11):38-40.