氨法制备低铁锌工艺研究
Process Study on Preparing Low Iron Zinc by Ammonia Method
摘要
图/表
参考文献
相似文献
本文已被:浏览 2711次   下载 24次
              
中文摘要: 采用NH3-NH4Cl-H2O体系浸出锌焙砂,经过锌粉两段净化,再电积出低铁金属锌。浸出时Fe、Ge、Si、As、Sb、Pb均进入浸出渣,而Zn,Cu、Cd等进入浸出液中。锌的平均浸出率90.8%,总回收率89.5%。得到的电锌产品中杂质元素Cu,Cd、Sb、As、Ni、Co、Pb和Fe含量≤0.0002%。
中文关键词: 低铁锌  氨  氯化铵  锌焙砂
Abstract:A process of preparing low iron zinc has been studied.The process includes: leaching zinc calcine with ammonia and ammonium chloride solution,purifying with two stage cross-flow and zinc electrowinning.In leaching stage,iron,germanium,silicon,arsenic,antimony and lead remained to stay at residue,but zinc,copper,cadmium dissolved.The average leaching ratio of zinc is 90.82% and total recovery ration of zinc is 89.44%.The impurities of copper,cadmium,antimony,arsenic,nickel,cobalt,lead and iron in zinc are lower than 0.0002%.
文章编号:     中图分类号:TF813    文献标志码:
基金项目:
颜炜 四川省会东铅锌矿,四川西昌615000
颜炜' target='_blank'>YAN Wei Huidong Lead-zinc Mine of Sichuan Province, Xichang 615000, China
引用文本:
颜炜.氨法制备低铁锌工艺研究[J].有色金属(冶炼部分),2007(3):15-19.
.Process Study on Preparing Low Iron Zinc by Ammonia Method[J].Nonferrous Metals (Extractive Metallurgy),2007(3):15-19.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号