本文已被:浏览 2730次 下载 25次
中文摘要: 利用某铅冶炼厂产生的烟灰,以硫酸为浸取剂,采用适当的添加剂使Zn浸出率达到99%,经除杂净化、碳酸氢铵沉淀制取了纯度大于98%的氧化锌,同时浸渣含Pb达到40%以上,可作为炼铅原料。考察了硫酸浓度、添加剂种类及加入量、温度等对浸出率的影响。
Abstract:The zinc ash of lead refinery is used as raw material and vitriol as leaching agent,the zinc leaching rate is 99%,then the zinc oxide with >98% purity is made by ammonium bicarbonate precipitation process.The following factors on the zinc leaching rate are discussed n detail: sulfuric acid concentration,additive and temperature,etc.
keywords: Zinc ash Additive Leaching residues Zinc oxide
文章编号: 中图分类号:TF813 文献标志码:
基金项目:
YANG Shao-wen CAO Yao-hua LI Qi GAO Zhao-guo
Zhengzhou Institute of Multipurpose Utilization of Mineral Resources, CAGS, Zhengzhou 450006, China
引用文本:
杨绍文,曹耀华,李琦,高照国.铅冶炼烟灰的综合利用[J].有色金属(冶炼部分),2007(3):13-14,19.
.Research on Multipurpose Utilization of Zinc Ash from Lead Metallurgy[J].Nonferrous Metals (Extractive Metallurgy),2007(3):13-14,19.
杨绍文,曹耀华,李琦,高照国.铅冶炼烟灰的综合利用[J].有色金属(冶炼部分),2007(3):13-14,19.
.Research on Multipurpose Utilization of Zinc Ash from Lead Metallurgy[J].Nonferrous Metals (Extractive Metallurgy),2007(3):13-14,19.

关注微信公众号