新疆洪海沟矿床酸法地浸采铀试验
张青林1, 黄群英1, 贾志远1, 陈立1, 范龙1, 周义朋2, 黎广荣2
(1.新疆中核天山铀业有限公司;2.东华理工大学)
Acid In-situ Uranium Leaching Trial at Honghaigou Deposit, Xinjiang
摘要
图/表
参考文献
相似文献
本文已被:浏览 1492次   下载 1198次
投稿时间:2024-06-11     修订日期:2024-06-19     录用日期:2024-06-20     网络发布日期:2024-07-09
中文摘要: 洪海沟矿床是我国新疆千吨铀矿大基地的重要后备资源。为确立该矿床开发的适宜浸出工艺,在前期实验室研究基础上,开展了“四注一抽”规模的酸法地浸采铀试验。结果表明:该矿床微酸和低酸浸出均未达到预期浸出效果,采用3.0~4.0 g/L酸度酸化、7.0~7.5 g/L酸度浸出是适宜工艺;300 mg/L剂量的H2O2能加速铀的浸出,但受限于溶出的Fe含量较低,氧化剂效能受限;尽管矿床碳酸盐含量不高,但浸出液Ca2+、SO42-持续增加易形成石膏沉淀导致抽注流量下降,需要在后续生产中予以关注。
Abstract:Honghaigou deposit is an important reserve resource for the base of kiloton uranium mine in Xinjiang, China. In order to establish a suitable leaching process for the development of the deposit, a "four-injection-one-extraction" scale acid in-situ leaching of uranium test was conducted based on previous laboratory research. The results show that both slightly acidic and low acidic leaching of the deposit are not feasible, and an acidification of 3.0—4.0 g/L and leaching of 7.0—7.5 g/L are suitable processes. The 300 mg/L dose of H2O2 can accelerate the leaching of uranium, but the low content of dissolved Fe limits the efficiency of the oxidant. Despite the low carbonate content of the deposit, the continuous increase of Ca2+ and SO42- in the solution is easy to form gypsum deposition and lead to decrease of extraction flow, which needs to be paid attention to in subsequent production.
文章编号:     中图分类号:    文献标志码:
基金项目:国家自然科学基金资助项目(42072285)
引用文本:
张青林,黄群英,贾志远,陈立,范龙,黎广荣,周义朋.新疆洪海沟矿床酸法地浸采铀试验[J].有色金属(冶炼部分),2024(8):105-112.
ZHANG Qinglin,HUANG Qunying,JIA Zhiyuan,CHEN Li,FAN Long,LI Guangrong,ZHOU Yipeng.Acid In-situ Uranium Leaching Trial at Honghaigou Deposit, Xinjiang[J].Nonferrous Metals (Extractive Metallurgy),2024(8):105-112.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号