中文摘要: 氰化尾渣是黄金氰化提金过程中产生的主要危险固体废弃物。以氰化尾渣为原料,利用其较高的铁品位,通过还原焙烧制备铁碳微电解填料,通过探究填料制备条件和降解条件对苯甲羟肟酸废水降解效果的影响,考察其用于处理苯甲羟肟酸废水的可行性。结果表明,最佳焙烧条件为:焙烧温度1 200 ℃、无烟煤用量20%、焙烧时间10 min;最佳降解条件为:铁碳微电解填料用量3.75 g/L、溶液pH=4,该条件下废水中的苯甲羟肟酸去除率可达80%以上。该方法不仅实现了氰化尾渣的资源化利用,而且可以有效降解苯甲羟肟酸废水,取得了“以废治废”的目的。
Abstract:Cyanide tailings are the main hazardous solid wastes produced in the process of gold cyanidation and gold extraction. Iron-carbon micro-electrolytic filler was prepared by reduction roasting from cyanide tailings with high iron grade. The feasibility of treating benzohydroxamic acid wastewater was investigated by exploring the influence of preparation conditions and degradation conditions of fillers on the degradation effect of benzohydroxamic acid wastewater. The results show that the removal rate of phenylhydroxamic acid in wastewater is 80% above under the optimum roasting conditions including roasting temperature of 1 200 ℃, anthracite consumption of 20%, and roasting time of 10 min, and the optimum degradation conditions including dosage of iron-carbon micro-electrolysis filler of 3.75 g/L and pH value of the solution of 4. This method not only realizes the resource utilization of cyanide tailings, but also effectively degrades benzohydroxamic acid wastewater, and achieved the purpose of "treating waste with waste".
文章编号:     中图分类号:    文献标志码:
基金项目:江西省主要学科学术技术带头人培养计划资助项目(20212BCJL23051);江西省重点研发计划项目(20203BBGL73232);江西理工大学清江优秀青年人才计划项目(JXUSTQJYX201806)
引用文本:
汪东芳,刘如春,韩梦婷,余文.氰化尾渣制备铁碳微电解填料及降解苯甲羟肟酸废水[J].有色金属(冶炼部分),2023(7):110-116.
WANG Dong-fang,LIU Ru-chun,HAN Meng-ting,YU Wen.Preparation of Iron-Carbon Micro-electrolysis Filler from Cyanide Tailings and Its Degradation Performance for Benzohydroxamic Acid Wastewater[J].Nonferrous Metals (Extractive Metallurgy),2023(7):110-116.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号