中文摘要: 针对氯化洗涤液采用“冷却结晶—铁粉置换—氧化除铁—中和沉锌”工艺实现金、银、铜、铅、锌多元素梯次回收,并产出置换渣、氢氧化锌和氯化铅产品。金、银、铜、铅、锌的回收率分别为99.3%、98.3%、97.8%、81.7%和95.3%。置换渣、氢氧化锌和氯化铅产品中金、银、铜、铅、锌的品位分别为1 462 g/t、26 945 g/t、29.8%、39.55%和35.2%。
Abstract:Au, Ag, Cu, Pb and Zn were comprehensively recovered from chloride solution by the process of cooling-crystallization, iron powder replacement, iron removal by oxidation, and zinc neutralization precipitation. Replacement residue, lead chloride and zinc hydroxide were produced in this process. Under the optimum conditions, recovery of Au, Ag, Cu, Pb and Zn is 99.3%, 98.3%, 97.8%, 81.7% and 95.3%, respectively. Au, Ag, Cu, Pb and Zn contents in products are 1 462 g/t, 26 945 g/t, 29.8%, 39.55% and 35.2%, respectively.
keywords: chloride solution iron powder replacement iron removal by oxidation zinc neutralization precipitation
文章编号: 中图分类号: 文献标志码:
基金项目:北京矿冶科技集团有限公司科研基金(YJT2017012)
| 作者 | 单位 | |
| 王为振* | 北京矿冶科技集团有限公司 | wangrdf1@163.com |
| 常耀超 | 北京矿冶科技集团有限公司 | |
| 黄海辉 | 北京矿冶科技集团有限公司 | |
| 徐晓辉 | 北京矿冶科技集团有限公司 | |
| 靳冉公 | 北京矿冶科技集团有限公司 |
| Author Name | Affiliation | |
| Wang Wei-zhen | Bgrimm Technology Group | wangrdf1@163.com |
| Chang Yao-chao | ||
| Huang Hai-hui | ||
| Xu Xiao-hui | ||
| Jin Ran-gong |
引用文本:
王为振,常耀超,黄海辉,徐晓辉,靳冉公.从氯化洗涤液中梯次回收各有价元素[J].有色金属(冶炼部分),2019(3):20-23.
Wang Wei-zhen,Chang Yao-chao,Huang Hai-hui,Xu Xiao-hui,Jin Ran-gong.Comprehensive Recovery of Valuable Elements from Chloride Solution[J].Nonferrous Metals (Extractive Metallurgy),2019(3):20-23.
王为振,常耀超,黄海辉,徐晓辉,靳冉公.从氯化洗涤液中梯次回收各有价元素[J].有色金属(冶炼部分),2019(3):20-23.
Wang Wei-zhen,Chang Yao-chao,Huang Hai-hui,Xu Xiao-hui,Jin Ran-gong.Comprehensive Recovery of Valuable Elements from Chloride Solution[J].Nonferrous Metals (Extractive Metallurgy),2019(3):20-23.

关注微信公众号