本文已被:浏览 2144次 下载 2358次
投稿时间:2017-12-20 修订日期:2017-12-25 录用日期:2017-12-26 网络发布日期:2018-05-17
投稿时间:2017-12-20 修订日期:2017-12-25 录用日期:2017-12-26 网络发布日期:2018-05-17
中文摘要: 采用碱性焙烧—浸出工艺处理高砷高锡阳极泥,考察了碱料比、焙烧温度、焙烧时间、液固比、浸出温度及浸出时间等对金属浸出率的影响。结果表明,优化条件为:碱料比0.9、焙烧温度600℃、焙烧时间2h、液固比3(mL/g)、浸出温度80 ℃、浸出时间2 h。在此条件下,碱性焙烧—浸出工艺能实现砷锡高效分离,砷的回收率高达95.2%,浸出渣含砷<0.5%,其它有价金属有效富集以便后续回收。
Abstract:High As and Sn bearing anode slime were treated by alkaline roasting and leaching. The effects of mass ratio of soda to anode slime, roasting temperature, roasting time, L/S, leaching temperature, and leaching time on leaching efficiency of metals were investigated. The results show that leaching rate of As is 95.2% and As content in leaching slag is 0.5% below under the optimum conditions including mass ratio of soda to anode slime of 0.9, roasting temperature of 600 ℃, roasting time of 2 h, L/S=3 mL/g, leaching temperature of 80 ℃, and leaching time of 2 h. Other valuable metals in anode slime are relatively enriched for further recycling.
keywords: high As and Sn bearing anode slime alkaline roasting separation of As and Sn valuable metals
文章编号: 中图分类号:TF81;X756 文献标志码:
基金项目:2015年省级财政技术研究与开发补助费用项目(粤财工[2015]639号);2017广东普通高校创新团队项目(2017GKCXTD004)
| 作者 | 单位 | |
| 王晓阳 | 广东环境保护工程职业学院 环境工程系 | xywang_gdhbxy@163.com |
| 王文祥* | 广东环境保护工程职业学院 环境工程系 广东省固体废弃物资源化与重金属污染控制工程技术研究中心 | wwxiang110@163.com |
| 方红生 | 广东省固体废弃物资源化与重金属污染控制工程技术研究中心 | |
| 莫越坚 | 广东省固体废弃物资源化与重金属污染控制工程技术研究中心 |
引用文本:
王晓阳,王文祥,方红生,莫越坚.高砷高锡阳极泥中砷锡分离工艺研究[J].有色金属(冶炼部分),2018(6):9-12.
WANG Xiao-yang,WANG Wen-xiang,FANG Hong-sheng,MO Yue-jian.Study on Separation of Arsenic and Tin from High As and Sn Bearing Anode Slime[J].Nonferrous Metals (Extractive Metallurgy),2018(6):9-12.
王晓阳,王文祥,方红生,莫越坚.高砷高锡阳极泥中砷锡分离工艺研究[J].有色金属(冶炼部分),2018(6):9-12.
WANG Xiao-yang,WANG Wen-xiang,FANG Hong-sheng,MO Yue-jian.Study on Separation of Arsenic and Tin from High As and Sn Bearing Anode Slime[J].Nonferrous Metals (Extractive Metallurgy),2018(6):9-12.

关注微信公众号