中文摘要: 采用新型贫化炉(Φ3.6 m×8.1 m),在熔炼温度分别是1 200 ℃、1 250 ℃,沉降时间分别为30 min、60 min,Fe/SiO2=1.7~1.9的条件下,考察了熔剂、硫化剂和还原剂等对渣贫化效果的影响。结果表明,在铜原始熔炼渣中加入SiO2、B2O3或CaF2时,可增加冰铜的沉降分离效果。而FeS的加入对铜的回收几乎没有影响,但它能够和氧反应产生工艺所需热量,还能减少尖晶石相和渣中铜的溶解。在优化的综合条件下,氧气与天然气比值控制在1.6时,弃渣含铜可达到0.26%。
Abstract:Effects of flux, vulcanizing agent and reductant on slag dilution in new-type Dilution Furnace were investigated under the conditions including smelting temperature of 1 200 ℃ and 1 250 ℃, settling time of 30 min and 60 min, and Fe/SiO2=1.7~1.9. The results show that addition of SiO2, B2O3 or CaF2 into original copper smelting slag can improve settling separation effect. Though no effect on copper recovery, addition of FeS can provide heat required by reaction with oxygen and reduce copper dissolution in spinel phase and slag. Copper content in discarded slag can be controlled at 0.26% under the optimum comprehensive conditions with ratio of oxygen to natural gas of 1.6.
文章编号: 中图分类号: 文献标志码:
基金项目:国家国际科技合作专项(2013DFA70620)
| 作者 | 单位 | |
| 边瑞民* | 东营方圆有色金属有限公司 山东.东营 257091 | brm6688@163.com |
| 王智 | 东营方圆有色金属有限公司 | |
| 魏传兵 | 东营方圆有色金属有限公司 | |
| 赵宝军 | 东营方圆有色金属有限公司 |
| Author Name | Affiliation | |
| BIAN Rui-min | Dongying Fangyuan Nonferrous Metals Co., Ltd | brm6688@163.com |
| WANG Zhi | ||
| WEI Chuan-bin | ||
| ZHAO Bao-jun |
引用文本:
边瑞民,王智,魏传兵,赵宝军.降低炼铜弃渣含铜技术的应用研究[J].有色金属(冶炼部分),2018(4):10-14.
BIAN Rui-min,WANG Zhi,WEI Chuan-bin,ZHAO Bao-jun.Application Study on Technology of Reducing Copper Content in Discarded Slag[J].Nonferrous Metals (Extractive Metallurgy),2018(4):10-14.
边瑞民,王智,魏传兵,赵宝军.降低炼铜弃渣含铜技术的应用研究[J].有色金属(冶炼部分),2018(4):10-14.
BIAN Rui-min,WANG Zhi,WEI Chuan-bin,ZHAO Bao-jun.Application Study on Technology of Reducing Copper Content in Discarded Slag[J].Nonferrous Metals (Extractive Metallurgy),2018(4):10-14.

关注微信公众号