中文摘要: 采用锌焙砂除镁法,即用过量的锌焙砂将开路溶液中的锌沉淀并回收,镁留在溶液中,从而达到了除镁的目的。与传统的石灰法相比,不需要添加其他元素,依靠锌焙砂就可以沉淀锌。在锌焙砂粒度22 μm、反应时间2.5 h、温度60 ℃、每立方米废电解液焙砂加入量2.3~2.6 t的条件下,沉锌后液锌含量低于1.5 g/L,锌回收率大于95%,镁开路效率达到80%。
Abstract:Zinc calcine was applied to remove magnesium from zinc solution. Excess zinc calcine was applied to precipitate zinc from solution and magnesium remained in solution. Compared with traditional lime method, this process has no other impurities to add. Zinc content in solution after precipitation is 1.5 g/L below with zinc recovery of 95% above, and magnesium removal rate is 80% under the conditions including grain size of zinc oxide of 22 μm, reaction time of 2.5 h, temperature of 60 ℃, and zinc oxide dosage of 2.3~2.6 t for one ton of waste electrolyte.
keywords: zinc solution purification Mg removal zinc calcine
文章编号: 中图分类号: 文献标志码:
基金项目:科技部国际合作项目(KY201502004)
| 作者 | 单位 | |
| 王洪刚* | 北京矿冶研究总院 | wanghonggang033@163.com |
| 刘三平 | 北京矿冶研究总院 | 370537373@qq.com |
| 王海北 | 北京矿冶研究总院 | whaibei_01@163.com |
| Author Name | Affiliation | |
| Wang Honggang | Beijing General Research Institute of mining and metallurgy | wanghonggang033@163.com |
| Liu Sanping | 370537373@qq.com | |
| wang haibei | whaibei_01@163.com |
引用文本:
王洪刚,刘三平,王海北.锌溶液除镁技术研究[J].有色金属(冶炼部分),2017(6):7-9.
Wang Honggang,Liu Sanping,wang haibei.Study on Removal of Magnesium from Zinc Solution[J].Nonferrous Metals (Extractive Metallurgy),2017(6):7-9.
王洪刚,刘三平,王海北.锌溶液除镁技术研究[J].有色金属(冶炼部分),2017(6):7-9.
Wang Honggang,Liu Sanping,wang haibei.Study on Removal of Magnesium from Zinc Solution[J].Nonferrous Metals (Extractive Metallurgy),2017(6):7-9.

关注微信公众号