中文摘要: 研究采用高温氯化工艺回收焙烧氰化尾渣中的有价金属。结果表明,在氯化钙添加量7%、1 100 ℃焙烧2 h的条件下,Au、Ag、Cu、Pb、Zn的挥发率分别达到97.52%、71.78%、85.92%、98.59%、93.81%。球团采用梯级烘干的干燥工艺,经40 min干燥后,干球团落下强度>10次/0.5 m,抗压强度90%>100 N,基本符合回转窑进料的强度要求。
Abstract:Recovery of valuable metals from roasting cyanidation residue by high temperature chloridizing was investigated. The results show that volatilization rate of Au, Ag, Cu, Pb and Zn is 97.52%, 71.78%, 85.92%, 98.59% and 93.81%, respectively under the conditions of CaCl2 addition of 7%, roasting temperature of 1 100 ℃, and roasting time of 2 h. Gradient drying process was adopted to prevent pellet bursting and after 40 min drying, falling strength of dry pellets is >10 times/0.5 m and compressive strength is 90%>100 N, both basically meeting the feeding requirement of rotary kiln.
keywords: cyanidation residue high temperature chloridizing valuable metals volatilization rate gradient drying
文章编号: 中图分类号: 文献标志码:
基金项目:国家高技术研究发展计划(863计划)项目(2011AA06A104)
| 作者 | 单位 | |
| 孙留根 | 北京矿冶研究总院 | sun_lg@bgrimm.com |
| 黄海辉* | 北京矿冶研究总院 | sea-hui@163.com |
| 徐晓辉 | 北京矿冶研究总院 | |
| 常耀超 | 北京矿冶研究总院 | |
| 韦其晋 | 北京矿冶研究总院 |
| Author Name | Affiliation | |
| SUN Liu-gen | Bei jing general research institute of mining DdDd metallurgy | sun_lg@bgrimm.com |
| HUANG Hai-hui | sea-hui@163.com | |
| XU Xiao-hui | ||
| CHANG Yao-chao | ||
| WEI Qi-jin |
引用文本:
孙留根,黄海辉,徐晓辉,常耀超,韦其晋.焙烧氰化尾渣回收有价金属试验[J].有色金属(冶炼部分),2017(2):15-18.
SUN Liu-gen,HUANG Hai-hui,XU Xiao-hui,CHANG Yao-chao,WEI Qi-jin.Study on Recovery of Valuable Metals from Roasting Cyanidation Residue[J].Nonferrous Metals (Extractive Metallurgy),2017(2):15-18.
孙留根,黄海辉,徐晓辉,常耀超,韦其晋.焙烧氰化尾渣回收有价金属试验[J].有色金属(冶炼部分),2017(2):15-18.
SUN Liu-gen,HUANG Hai-hui,XU Xiao-hui,CHANG Yao-chao,WEI Qi-jin.Study on Recovery of Valuable Metals from Roasting Cyanidation Residue[J].Nonferrous Metals (Extractive Metallurgy),2017(2):15-18.

关注微信公众号