本文已被:浏览 2052次 下载 2370次
投稿时间:2016-06-20 修订日期:2016-06-28 录用日期:2016-07-04 网络发布日期:2016-11-17
投稿时间:2016-06-20 修订日期:2016-06-28 录用日期:2016-07-04 网络发布日期:2016-11-17
中文摘要: 某浸染型沥青铀矿石在酸法搅拌浸出条件下,-0.104 mm粒度矿石铀的浸出率不到50%。采用“拌酸熟化预处理—高余酸浸出”工艺,-20 mm矿石拌酸柱浸铀的浸出率大于83%,浸出尾渣铀品位低于0.01%。
浸出液采用离子交换吸附、酸性氯化钠淋洗、淋洗液沉淀工艺制备铀产品,吸附的树脂铀负载容量达到125 mg/g,淋洗液铀浓度10 g/L以上,沉淀的"111"产品达到行业一级品要求。
Abstract:Uranium extraction rate of impregnated pitchblende uranium ore with particle size of -0.104 mm is 50% below under acid leaching. Uranium column leaching rate is 83% above and tailing grade of uranium is 0.01% below with particle size of -0.20 mm applying processes of mixed acid-curing pretreatment and high acid leaching. Lixivium was treated by ion exchange adsorption, acidic sodium chloride leaching, and uranium precipitation to produce uranium product. Adsorption capacity of uranium is 125 mg/g. Uranium concentration of leacheate is 10 g/L above. The product of precipitant “111” meets the requirements of standard of First Class of industry.
keywords: uranium ore pitchblende acid-curing leaching
文章编号: 中图分类号: 文献标志码:
基金项目:无
| 作者 | 单位 | |
| 王高山 | 核工业北京化工冶金研究院 | wanggao_3@163.com |
| 张黎辉* | 环境保护部核与辐射安全中心 | dyzhlh@126.com |
| 李铁球 | 核工业北京化工冶金研究院 | |
| 王聪颖 | 核工业北京化工冶金研究院 | |
| 刘津麟 | 核工业北京化工冶金研究院 | |
| 童长宁 | 中国核工业集团公司抚州金安铀业有限公司 |
引用文本:
王高山,张黎辉,李铁球,王聪颖,刘津麟,童长宁.浸染型沥青铀矿石水冶工艺研究[J].有色金属(冶炼部分),2016(12):51-55.
WANG Gao-shan,ZHANG Li-hui,li tieqiu,wang congying,LIU Jin-lin,TONG Chang-ning.Study on Hydrometallurgy of Impregnated Pitchblende Uranium Ore[J].Nonferrous Metals (Extractive Metallurgy),2016(12):51-55.
王高山,张黎辉,李铁球,王聪颖,刘津麟,童长宁.浸染型沥青铀矿石水冶工艺研究[J].有色金属(冶炼部分),2016(12):51-55.
WANG Gao-shan,ZHANG Li-hui,li tieqiu,wang congying,LIU Jin-lin,TONG Chang-ning.Study on Hydrometallurgy of Impregnated Pitchblende Uranium Ore[J].Nonferrous Metals (Extractive Metallurgy),2016(12):51-55.

关注微信公众号