中文摘要: 研究了硫化锑与氧化锌在Na2CO3-NaCl熔盐体系中的还原固硫直接炼锑反应机理。热力学计算表明,硫化锑与氧化锌的还原固硫反应在400 ℃以上可自发进行,在熔体中x(Sb2S3)和x(ZnO)都降至0.000 1时,碳气化反应的CO%也可满足还原所需的平衡气氛要求。在Sb2S3-ZnO-C体系中,硫化锑还原固硫反应分两步进行:Sb2S3首先与ZnO发生交互反应生成Sb2O3和ZnS,Sb2O3再被还原剂C或CO还原成Sb,从而以ZnS形式实现固硫。
Abstract:Reaction mechanism of antimony direct smelting by reduction and sulfur-fixing reaction between Sb2S3 and ZnO in Na2CO3-NaCl molten salt was investigated. The results of thermodynamic calculation indicate that sulfur-fixing reaction can completely proceed at 400 ℃ above, CO% from gasification reaction of carbon can meet reduction and sulfur-fixing reaction even when mole concentration of Sb2S3 and ZnO in melt is both as low as 0.0001. In Sb2S3-ZnO-C system, sulfur-fixing reaction is divided into two steps, reaction between Sb2S3 and ZnO to produce Sb2O3 and ZnS firstly, and then consecutive reduction of Sb2O3 to Sb by addition of reductive agent. SO2 smoke is discharged in form of ZnS.
keywords: antimony metallurgy sulfur-fixation smelting reaction mechanism low temperature molten salt
文章编号: 中图分类号:TF818 文献标志码:
基金项目:国家自然科学基金资助项目(51104182)
引用文本:
王岳俊,陈永明,徐康宁,叶龙刚,薛浩天,王彩虹.辉锑矿锌源固硫直接炼锑反应机理研究[J].有色金属(冶炼部分),2016(10):1-4.
WANG Yue-jun,CHEN Yong-ming,XU Kang-ning,YE Long-gang,Xue Hao-tian,WANG Cai-hong.Reaction Mechanism of Antimony Direct Smelting Applying Zinc Materials as Sulfur-fixing Agent[J].Nonferrous Metals (Extractive Metallurgy),2016(10):1-4.
王岳俊,陈永明,徐康宁,叶龙刚,薛浩天,王彩虹.辉锑矿锌源固硫直接炼锑反应机理研究[J].有色金属(冶炼部分),2016(10):1-4.
WANG Yue-jun,CHEN Yong-ming,XU Kang-ning,YE Long-gang,Xue Hao-tian,WANG Cai-hong.Reaction Mechanism of Antimony Direct Smelting Applying Zinc Materials as Sulfur-fixing Agent[J].Nonferrous Metals (Extractive Metallurgy),2016(10):1-4.

关注微信公众号