中文摘要: 对某难处理金矿热压氧化渣进行炭浸氰化试验,考察pH、调浆时间、底炭浓度、氰化钠初始浓度、浸出时间对金浸出率的影响。结果表明,在下述最佳条件下,氰化钠的消耗仅为0.27~0.29 kg/t,金浸出率为95.34%:底炭浓度60 kg/t、氧化钙用量35 kg/t、氰化钠初始浓度1.5 kg/t、调浆时间2 h、室温浸出2~4 h。难处理金矿经过热压氧化预处理后炭浸法提金,具有浸出反应动力学快,浸出率高,氰化钠消耗低的特点。
Abstract:Residue of refractory gold ore after pressure oxidation pretreatment was leached by carbon-in-leach (CIL). Effects of pH, slurry-mixing time, active carbon concentration, initial concentration of NaCN, and leaching time on gold leaching rate were investigated. The results show that gold leaching rate is 95.34% with NaCN consumption of 0.27~0.29 kg/t under the optimum conditions including active carbon concentration of 60 kg/t, CaO consumption of 35 kg/t, initial concentration of NaCN of 1.5 kg/t, slurry-mixing time of 2 h, and leaching duration of 2~4 h at room temperature. This process has the advantages of fast reaction kinetics, high gold leaching rate, and low consumption of NaCN.
文章编号: 中图分类号:TF831 文献标志码:
基金项目:广西科学研究与技术开发计划项目(桂科攻14122006-25);中国有色集团科技计划项目(2014KJJH02)
| 作者 | 单位 | |
| 罗 星* | 中国有色桂林矿产地质研究院有限公司 | luojiexing304@163.com |
| 李尽善 | 中国有色桂林矿产地质研究院有限公司 | |
| 周卫宁 | 中国有色桂林矿产地质研究院有限公司 | |
| 冯吉福 | 中国有色桂林矿产地质研究院有限公司 | |
| 马荣锴 | 中国有色桂林矿产地质研究院有限公司 |
| Author Name | Affiliation | |
| LUO Xing | China Nonferrous Metal Guilin Geology and Mining Co. Ltd. | luojiexing304@163.com |
| LI Jinshan | ||
| ZHOU Weining | ||
| FENG Jifu | ||
| MA Rongkai |
引用文本:
罗 星,李尽善,周卫宁,冯吉福,马荣锴.某金矿预处理后碳浸法提金试验[J].有色金属(冶炼部分),2016(9):28-30.
LUO Xing,LI Jinshan,ZHOU Weining,FENG Jifu,MA Rongkai.Research on Carbon-in-Leaching of Gold Ore after Pretreatment[J].Nonferrous Metals (Extractive Metallurgy),2016(9):28-30.
罗 星,李尽善,周卫宁,冯吉福,马荣锴.某金矿预处理后碳浸法提金试验[J].有色金属(冶炼部分),2016(9):28-30.
LUO Xing,LI Jinshan,ZHOU Weining,FENG Jifu,MA Rongkai.Research on Carbon-in-Leaching of Gold Ore after Pretreatment[J].Nonferrous Metals (Extractive Metallurgy),2016(9):28-30.

关注微信公众号