中文摘要: 采用氢氧化钠碱浸回收电解锰阳极泥中的硒,考察氢氧化钠浓度、浸出温度、液固比、浸出时间和搅拌速度等对硒浸出率的影响,并在此基础上研究了超声辅助强化浸出的效果。结果表明,超声辅助强化浸出可以降低浸出温度,缩短反应时间,并能有效提高硒的浸出率。当超声功率为500 W时,60 ℃反应50 min,硒的浸出率达到96.11%。
Abstract:Selenium was recycled from electrolytic manganese anode slime by alkaline leaching. The effects of sodium hydroxide concentration, leaching temperature, ratio of liquid to solid, leaching time and stirring speed on selenium leaching rate were investigated. The ultrasonic extraction experiments were applied to reinforce alkaline leaching based on the result of single factor experiments. The results show that ultrasonic extraction can improve selenium leaching rate, reduce leaching temperature and time. Selenium leaching rate is 96.11% under the conditions including ultrasonic power of 500 W, ultrasonic time of 50 min, and temperature of 60 ℃.
文章编号: 中图分类号:TQ137.1 文献标志码:
基金项目:广西科技开发计划项目(桂科转1599002-4,桂科能1598026-10);广西研究生教育创新计划项目(YCBZ2014014)
| 作者 | 单位 | |
| 曾宪日* | 广西大学化学化工学院 | zengxianri 1991@163.com |
| 王雨红 | 广西大学化学化工学院 | |
| 屈欣轲 | 广西大学化学化工学院 | |
| 何旻雁 | 广西大学化学化工学院 | |
| 粟海锋 | 广西大学化学化工学院 | suhfeng@gxu.edu.cn |
| Author Name | Affiliation | |
| ZENG Xian-ri | College of Chemistry and Chemical Engineering,Guangxi University | zengxianri 1991@163.com |
| WANG Yu-hong | ||
| QU Xin-ke | ||
| HE Min-yan | ||
| SU Hai-feng | suhfeng@gxu.edu.cn |
引用文本:
曾宪日,王雨红,屈欣轲,何旻雁,粟海锋.碱浸回收电解锰阳极泥中硒的研究[J].有色金属(冶炼部分),2016(8):48-51.
ZENG Xian-ri,WANG Yu-hong,QU Xin-ke,HE Min-yan,SU Hai-feng.Selenium Recovery from Manganese Anode Slime by Alkaline Leaching[J].Nonferrous Metals (Extractive Metallurgy),2016(8):48-51.
曾宪日,王雨红,屈欣轲,何旻雁,粟海锋.碱浸回收电解锰阳极泥中硒的研究[J].有色金属(冶炼部分),2016(8):48-51.
ZENG Xian-ri,WANG Yu-hong,QU Xin-ke,HE Min-yan,SU Hai-feng.Selenium Recovery from Manganese Anode Slime by Alkaline Leaching[J].Nonferrous Metals (Extractive Metallurgy),2016(8):48-51.

关注微信公众号