本文已被:浏览 2817次 下载 2376次
投稿时间:2014-12-25 修订日期:2015-01-04 录用日期:2015-01-05 网络发布日期:2015-05-20
投稿时间:2014-12-25 修订日期:2015-01-04 录用日期:2015-01-05 网络发布日期:2015-05-20
中文摘要: 采用酸浸—高温氯化工艺对高砷硫酸烧渣进行脱砷和回收金银。结果表明,在硫酸浓度30 g/L、酸浸渣磨矿粒度-0.037 mm占81.87%、CaCl2加入量5%、膨润土加入量2%、焙烧温度1 200 ℃、焙烧时间2 h的最佳条件下,球团中铁品位达到55%以上,金、银挥发率分别为90.8%、82.4%,球团中As、S、Cu、Pb、Zn等杂质含量分别为0.32%、0.011%、0.057%、0.11%、0.38%。球团强度基本在2.5 kN以上。脱砷酸浸液中硫化钠加入量达到3倍理论量(30 kg/m3)时,砷的沉淀率达到96.7%。
Abstract:Acid leaching-high temperature chlorination process is used to remove arsenic and recover gold and silver from high arsenic-bearing pyrite cinder. The results show that iron grade in roasted pellet is 55% above, contents of As, S, Cu, Pb, Zn in pellet are 0.32%, 0.011%, 0.057%, 0.11%, and 0.38% respectively under the optimum conditions including sulfuric acid concentrate of 30 g/L, particle size of -0.037 mm of 81.87%, dosage of CaCl2 of 5%, bentonite dosage of 2%, roasting temperature of 1 200 ℃, and roasting time of 2h. Roasted pellet intensity is 2.5 kN above. Arsenic deposition rate is 96.7% when Na2S addition is three times of theoretical amount.
文章编号: 中图分类号: 文献标志码:
基金项目:国家高技术研究发展计划(863计划)项目(2011AA06A104)
| 作者 | 单位 | |
| 常耀超* | 北京矿冶研究总院冶金所 | chang_yc@bgrimm.com |
| 徐晓辉 | 北京矿冶研究总院冶金所 | |
| 王云 | 北京矿冶研究总院工程公司 |
| Author Name | Affiliation | |
| Chang Yaochao | Beijing General Research Institute of Mining Metallurgy | chang_yc@bgrimm.com |
| Xu Xiaohui | ||
| Wang Yun |
引用文本:
常耀超,徐晓辉,王云.高砷硫酸烧渣脱砷及高温氯化回收金银[J].有色金属(冶炼部分),2015(6):46-49.
Chang Yaochao,Xu Xiaohui,Wang Yun.Arsenic Removal and Recovery of Gold and Silver by Chloridizing Roasting from High Arsenic-bearing Pyrite Cinder[J].Nonferrous Metals (Extractive Metallurgy),2015(6):46-49.
常耀超,徐晓辉,王云.高砷硫酸烧渣脱砷及高温氯化回收金银[J].有色金属(冶炼部分),2015(6):46-49.
Chang Yaochao,Xu Xiaohui,Wang Yun.Arsenic Removal and Recovery of Gold and Silver by Chloridizing Roasting from High Arsenic-bearing Pyrite Cinder[J].Nonferrous Metals (Extractive Metallurgy),2015(6):46-49.

关注微信公众号