中文摘要: 采用以重金属吸附材料为基础的连续交换技术,对离子型稀土矿浸出母液分别进行杂质分离和稀土富集试验。结果表明,解吸液中稀土含量大于100 g/L,富集了约200倍,稀土对铝的比值约176.4∶1,稀土对铁的比值约568.3∶1。此工艺可简化离子型稀土矿浸出母液浓缩工艺流程,提升稀土浓缩液品质,降低成本。
Abstract:Impurity separation and rare earth enrichment were conducted on the mother lixivium of ion-type rare earth ore by continuous adsorption and exchange technology based on heavy metal adsorption material. The results show that the rare earth concentration in desorption solution is above 100 g/L with the enrichment improved by about 200 times. The ratio of rare earth to aluminum and iron is 176.4∶1 and 568.3∶1 respectively. This process can simplify enrichment process of mother lixivium of ion-type rare earth ore, improve quality of concentrated rare earth solution and reduce cost.
keywords: heavy metal adsorption material continuous adsorption and exchange ion-type rare earth ore lixivium new concentration process
文章编号: 中图分类号: 文献标志码:
基金项目:
| 作者 | 单位 | |
| 邱建宁 | 工信华鑫科技集团 | qiujianing@iihxt.com |
| 林楚浩 | 工信华鑫科技集团 | |
| 田春友 | 工信华鑫科技集团 | |
| 葛鹏* | 工信华鑫科技集团 | garudakeh@163.com |
| 潘勇进 | 工信华鑫科技集团 |
| Author Name | Affiliation | |
| Qiu Jian-ning | Gongxin Huaxin Technology Group | qiujianing@iihxt.com |
| Lin Chu-hao | ||
| Tian Chun-you | ||
| Ge Peng | garudakeh@163.com | |
| Pan Yong-jin |
引用文本:
邱建宁,林楚浩,田春友,葛鹏,潘勇进.离子型稀土矿浸出母液新型浓缩工艺[J].有色金属(冶炼部分),2014(3):40-41.
Qiu Jian-ning,Lin Chu-hao,Tian Chun-you,Ge Peng,Pan Yong-jin.New Concentration Process of Mother Lixivium of Ion-type Rare Earth Ore[J].Nonferrous Metals (Extractive Metallurgy),2014(3):40-41.
邱建宁,林楚浩,田春友,葛鹏,潘勇进.离子型稀土矿浸出母液新型浓缩工艺[J].有色金属(冶炼部分),2014(3):40-41.
Qiu Jian-ning,Lin Chu-hao,Tian Chun-you,Ge Peng,Pan Yong-jin.New Concentration Process of Mother Lixivium of Ion-type Rare Earth Ore[J].Nonferrous Metals (Extractive Metallurgy),2014(3):40-41.

关注微信公众号