中文摘要: 锌冶炼净化渣先进行高温浸出,使锌、钴、镉等有价金属进入浸出液,而铜留在渣中,所得铜渣再经高酸浸出及水洗后得到铜精矿。结果表明,最佳高温浸出条件为:液固比(6~7)∶1,始酸浓度100 g/L、终点pH=3.0、80~85 ℃浸出8 h;高酸洗涤最佳条件为:液固比(4~6)∶1,终点酸度50 g/L,70~80 ℃浸出60~90 min。铜精矿含铜65%以上、含锌小于2%。
中文关键词: 湿法炼锌  净化渣  酸性浸出  洗涤  铜精矿
Abstract:The purification slag from zinc hydrometallurgy was first leached at high temperature. Valuable metals of zinc, cobalt and cadmium entered into lixivium, and copper remained in slag. Copper concentrate was obtained from this copper slag by high acidic leaching and washing process. The results show that copper concentrate with copper grade of 65% above and less than 2% of zinc is obtained under the optimum high temperature leaching conditions including ratio of solid to liquid of (6~7)∶1, original acid concentration of 100 g/L, pH value of terminal point of 3.0, temperature of 80~85 ℃, and time of 8 h and the optimum high acidic washing conditions including ratio of solid to liquid of (4~6)∶1, terminal acidity of 50 g/L, temperature of 70~87 ℃, and time of 60~90 min.
文章编号:     中图分类号:    文献标志码:
基金项目:
引用文本:
郭新玲.从锌冶炼净化渣中回收高品位铜精矿[J].有色金属(冶炼部分),2013(10):4-6.
guoxinling.Recovery of High Grade Copper Concentrate from Purification Slag of Zinc Hydrometallurgy[J].Nonferrous Metals (Extractive Metallurgy),2013(10):4-6.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号