中文摘要: 采用针铁矿法除去萃铜后的铜钴矿细菌浸出液中的铁,并对除铁时的pH、氧化剂浓度、氧化时间、保温时间等因素进行优化。结果表明,控制氧化过程中pH为4.0、氧化温度70 ℃、保温时间1 h、氧化剂浓度8%,除铁率和钴回收率分别为99.9%和99.5%。针铁矿法除铁可以在常压和较低温度(70 ℃)下进行,而且不需外加其他金属阳离子就能获得过滤性能良好且可作为含铁富矿使用的沉淀渣。
Abstract:The iron was removed from Cu-Co ore bioleaching solution after copper extraction with goethite process. The parameters of pH value, concentration of oxidant, oxidation time and deironization time were optimized. The results show that the iron removal rate and cobalt recovery rate are 99.9% and 99.5% respectively under the optimum conditions including pH of 4.0, oxidation temperature of 70 ℃, holding time of 1 h, and concentration of oxidant of 8%. The goethite deironization process can be conducted at atmospheric pressure, low temperature (70 ℃) and without addition of other metal ions. The precipitation slag is rich of iron and has good filterability.
文章编号: 中图分类号: 文献标志码:
基金项目:国家高技术研究发展计划项目(2012AA061501; 2012AA061502);中央高校基本科研业务费项目(N110302002)
| 作者 | 单位 | |
| 陈国宝* | 东北大学材料与冶金学院 | cgb8922@163.com |
| 杨洪英 | 东北大学材料与冶金学院 | |
| 周立杰 | 东北大学材料与冶金学院 | |
| 李海军 | 东北大学材料与冶金学院 |
| Author Name | Affiliation | |
| Guobao Chen | School of Materials Metallurgy,Northeastern University | cgb8922@163.com |
| Hongying Yang | ||
| Lijie zhou | ||
| Haijun Li |
引用文本:
陈国宝,杨洪英,周立杰,李海军.针铁矿法从铜钴矿生物浸出液中除铁的研究[J].有色金属(冶炼部分),2013(3):1-3.
Guobao Chen,Hongying Yang,Lijie zhou,Haijun Li.Study on Goethite Deironization from Bioleaching Solution of Cu-Co Ore[J].Nonferrous Metals (Extractive Metallurgy),2013(3):1-3.
陈国宝,杨洪英,周立杰,李海军.针铁矿法从铜钴矿生物浸出液中除铁的研究[J].有色金属(冶炼部分),2013(3):1-3.
Guobao Chen,Hongying Yang,Lijie zhou,Haijun Li.Study on Goethite Deironization from Bioleaching Solution of Cu-Co Ore[J].Nonferrous Metals (Extractive Metallurgy),2013(3):1-3.

关注微信公众号