中文摘要: 针对某氧化钼钨粗精矿高压碱浸后得到的浸出液钼钨含量均较高、钼钨分离困难的特点,确定了钼钨浸出液镁盐净化除杂、钼钨共沉淀、干燥、钼钨酸铵制备的工艺流程,主要考察了氯化铵用量、沉淀时间、pH、温度、溶液浓度对钼沉淀率的影响。结果表明,最终获得的产品含Mo 47.57%、WO3 10.13%,杂质磷、砷分别为0.0027%、0.041%,产品符合生产钨钼合金的要求。
Abstract:According to the characteristics of high tungsten and molybdenum content in the high pressure leaching solution of tungsten and molybdenum oxide rough concentrate, a new process for molybdenum-tungsten extraction was adopted including purification with magnesium salt, molybdenum-tungsten co-precipitation, drying, preparation of ammonium molybdate-tungstate. The effects of ammonium chloride dosage, precipitation time, pH, temperature, and solution concentration on molybdenum precipitation rate were investigated. The results show that the final products, i.e., ammonium molybdate-tungstate, contain 47.57% Mo and 10.13% WO3, respectively, and the impurities of phosphorus and arsenic are 0.0027% and 0.041%, respectively. This product meets requirement of molybdenum-tungsten alloy production.
文章编号: 中图分类号: 文献标志码:
基金项目:
| 作者 | 单位 | |
| 曹耀华* | 中国地质科学院郑州矿产综合利用研究所 | cao2078@126.com |
| 刘红召 | 中国地质科学院郑州矿产综合利用研究所 | hongzhao99@126.com |
| 高照国 | 中国地质科学院郑州矿产综合利用研究所 | 1269758113@99.com |
| 杨绍文 | 中国地质科学院郑州矿产综合利用研究所 | zzsrsc@126.com |
引用文本:
曹耀华,刘红召,高照国,杨绍文.从高压碱浸液中提取钼钨新工艺[J].有色金属(冶炼部分),2012(10):27-29.
caoyaohua,liuhongzhao,gaozhaoguo,yangshaowen.New Process for Molybdenum and Tungsten Extraction from High Pressure Alkaline Leaching Solution[J].Nonferrous Metals (Extractive Metallurgy),2012(10):27-29.
曹耀华,刘红召,高照国,杨绍文.从高压碱浸液中提取钼钨新工艺[J].有色金属(冶炼部分),2012(10):27-29.
caoyaohua,liuhongzhao,gaozhaoguo,yangshaowen.New Process for Molybdenum and Tungsten Extraction from High Pressure Alkaline Leaching Solution[J].Nonferrous Metals (Extractive Metallurgy),2012(10):27-29.

关注微信公众号