中文摘要: 采用氯化挥发法在马弗炉和管式炉中处理含锡尾矿,探索还原剂(无烟煤)和氯化剂(CaCl2)的加入量对有价金属挥发的影响。结果表明,在无烟煤加入量8%,氯化钙加入量21%,石灰加入量5.21%,温度1 000 ℃,挥发时间3 h的条件下,锡挥发率达到96.15%,铅和锌的挥发率分别为96.22%和73.51%。
Abstract:Tin tailings were chloride volatilized in Muffle furnace and pipe furnace. The effects of reductant (anthracite) and calcium chloride on volatility of valuable metals were investigated. The results show that the volatility rates of tin, lead and zinc are 96.15%, 96.22% and 73.51%, respectively under the following optimum conditions including anthracite dosage of 8%, calcium chloride dosage of 21%, lime dosage of 5.21%, temperature of 1 000 ℃, and time of 3 hours.
keywords: tin tailings chlorination volatility rate tin lead zinc
文章编号: 中图分类号: 文献标志码:
基金项目:
| Author Name | Affiliation | |
| Li Xue-peng | Institute of Research & Designing of YTC | jack56_2009@126.com |
| Yin Jiu-fa |
引用文本:
李学鹏,尹久发.氯化挥发回收含锡尾矿中的有价金属[J].有色金属(冶炼部分),2012(9):11-14.
Li Xue-peng,Yin Jiu-fa.Valuable Metals Recovery from Tin Tailing with Chlorination Volatility Process[J].Nonferrous Metals (Extractive Metallurgy),2012(9):11-14.
李学鹏,尹久发.氯化挥发回收含锡尾矿中的有价金属[J].有色金属(冶炼部分),2012(9):11-14.
Li Xue-peng,Yin Jiu-fa.Valuable Metals Recovery from Tin Tailing with Chlorination Volatility Process[J].Nonferrous Metals (Extractive Metallurgy),2012(9):11-14.

关注微信公众号