低砷次氧化锌烟尘综合回收工艺研究
易超,鲁兴武,马爱军
(西北矿冶研究院冶金新材料研究所,西北矿冶研究院冶金新材料研究所,西北矿冶研究院冶金新材料研究所)
Study on Comprehensive Recovery of Low Arsenic Secondary Zinc Oxide Dust
Yi Chao,Lu Xingwu and Ma Aijun
(Northwest Institute of Mining and Metallurgy,,)
摘要
图/表
参考文献
相似文献
本文已被:浏览 2500次   下载 2261次
投稿时间:2012-01-02     修订日期:2012-01-02     录用日期:2012-01-05     网络发布日期:2012-07-25
中文摘要: 对锌冶炼含铟窑渣综合回收新工艺进行优化,考察了酸度、液固比、时间、温度等因素对锌和铟浸出率的影响以及不同酸度下金属铟的走向,得到最优工艺条件。在二段浸出后铟综合回收率为82.8%。
中文关键词: 次氧化锌  铟  浸出  优化  回收率
Abstract:A new comprehensive recovery process from zinc smelting slag with indium content was optimized. The effects of acidity, ratio of liquid to solid, time, temperature on the leaching rate of zinc and indium were investigated, and whereabouts of metal indium with a variety of acidity were studied. The optimal process conditions were obtained. The results show that the overall recovery of indium is 82.8% after two step leaching.
文章编号:     中图分类号:    文献标志码:
基金项目:青海省重大科技攻关项目(2006-G-157)
引用文本:
易超,鲁兴武,马爱军.低砷次氧化锌烟尘综合回收工艺研究[J].有色金属(冶炼部分),2012(8):7-10.
Yi Chao,Lu Xingwu,Ma Aijun.Study on Comprehensive Recovery of Low Arsenic Secondary Zinc Oxide Dust[J].Nonferrous Metals (Extractive Metallurgy),2012(8):7-10.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号