铁闪锌矿低温加压浸出过程中锌、硫、铁的行为
徐志峰,江庆政,王成彦
(江西理工大学 冶金与化学工程学院,江西理工大学 冶金与化学工程学院,北京矿冶研究总院)
Behavior of Zinc, Sulfur and Iron in Low-temperature Pressure Leaching Process of Marmatite
XU Zhi-feng,JIANG Qing-zheng and WANG Cheng-yan
(School of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology,,)
摘要
图/表
参考文献
相似文献
本文已被:浏览 2948次   下载 2837次
投稿时间:2011-12-31     修订日期:2011-12-31     录用日期:2012-01-04     网络发布日期:2012-06-26
中文摘要: 以人工合成的高纯度铁闪锌矿为研究对象,基于对388 K温度条件下浸出过程物相及矿物表面性质变化的分析,研究锌、硫、铁等元素的低温加压浸出行为。结果表明,元素锌仅发生溶解反应而且溶解锌能稳定存在于水溶液中;浸出初期,铁闪锌矿电化学氧化反应滞后,而铁闪锌矿酸溶反应才是浸出初期最主要的化学反应,浸出初期无SO42-氧化生成,但在浸出后期,可能有少量单质硫进一步氧化生成SO42-。单质硫是铁闪锌矿最主要的氧化产物;浸出过程中,铁溶出与溶解铁的水解沉淀反应是同步进行的。在浸出初期,铁的溶出占主导地位,而在浸出后期,溶解铁的水解沉淀则是主要反应而且铁的沉淀形态可以调控。
中文关键词: 铁闪锌矿  低温加压浸出  锌  硫  铁  浸出行为
Abstract:The low-temperature pressure leaching of synthesized marmatite was studied. The leaching behavior of zinc, sulfur and iron was discussed based on the analysis of the phase change and the mineral surface properties at 388 K. The results indicate that only the dissolving reaction takes place for zinc and the dissolved zinc can exist in the solution stably. The acidic dissolving of marmatite, other than the electrochemical oxidation is the main chemical reaction in the initial leaching. No sulfate ion is produced in the initial leaching while a small quantity of elemental sulfur is further oxidized into sulfate in the terminal leaching. Elemental sulfur is the main oxidization product of marmatite. The dissolving and hydrolysis precipitation of iron occur simultaneously in the leaching. In term of iron, the dissolving is the main reaction in the initial leaching while the hydrolysis precipitation is predominant in the terminal leaching and the form of precipitates can be controlled.
文章编号:     中图分类号:    文献标志码:
基金项目:国家自然科学基金资助项目(50964004);江西省第四批青年科学家培养对象资助项目(赣科发计字[2010]209号)
引用文本:
徐志峰,江庆政,王成彦.铁闪锌矿低温加压浸出过程中锌、硫、铁的行为[J].有色金属(冶炼部分),2012(7):6-11.
XU Zhi-feng,JIANG Qing-zheng,WANG Cheng-yan.Behavior of Zinc, Sulfur and Iron in Low-temperature Pressure Leaching Process of Marmatite[J].Nonferrous Metals (Extractive Metallurgy),2012(7):6-11.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号