有色金属(冶炼部分):2011,(11):6-8
本文二维码信息
码上扫一扫!
硫酸烧渣加压浸取铁
(东华大学环境科学与工程学院)
Pressure Reduction Leaching Iron from Sulfate Slag
(School of Environmental Science and Engineering, Donghua University)
摘要
图/表
参考文献
相似文献
本文已被:浏览 3335次   下载 39次
投稿时间:2011-03-26               
中文摘要: 采用自制硫化物助浸剂在密闭反应釜中还原浸出硫酸烧渣中的高铁。分别进行了助浸剂用量、硫酸用量、始酸浓度、反应温度、搅拌速度、反应时间等条件试验,考察各因素对浸取效果的影响。结果表明:当酸浸渣25.0 g,助浸剂过剩系数1.1,硫酸过剩系数1.4,始酸浓度3.5 mol/L,反应温度95 ℃,搅拌速度800 r/min,反应时间3 h时,铁浸取率达99.4%,助浸剂有效利用率达98.9%。
中文关键词: 硫酸烧渣  高铁  助浸剂  硫化物
Abstract:Ferric iron was reduction leached from sulfate slag with sulfide agent. Effects of the following factors on leaching were studied, such as, dosage of additives, sulfuric acid consumption, initial sulfuric acid concentration, reaction temperature, stirring speed, and reaction time. The results show that iron leaching rate reaches 99.4%, efficiency of additive usage reaches 98.9% on the following conditions: surplus coefficient of leaching agent is 1.1, surplus coefficient of sulfuric acid is 1.4, 3.5 mol/L initial sulfuric acid concentration with 800 r/min stirring rate, 95 ℃, 3 h.
文章编号:     中图分类号:    文献标志码:
基金项目:国家高技术研究发展计划(863)资助项目(2006AA06Z132);上海市重点学科建设资助项目(B604)
引用文本:
金程.硫酸烧渣加压浸取铁[J].有色金属(冶炼部分),2011(11):6-8.
JIN Cheng.Pressure Reduction Leaching Iron from Sulfate Slag[J].Nonferrous Metals (Extractive Metallurgy),2011(11):6-8.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号