有色金属(冶炼部分):2011,(12):11-14
←前一篇   |   后一篇→
本文二维码信息
码上扫一扫!
含砷金矿提金渣综合回收砷
(四川大学化学工程学院)
Comprehensive Recovery of Arsenic from Gold Ore Slag
(College of Chemical Engineering, Sichuan University, Chengdu 610065, China)
摘要
图/表
参考文献
相似文献
本文已被:浏览 3466次   下载 40次
投稿时间:2011-05-24               网络发布日期:2011-12-06
中文摘要: 以细菌氧化提金废渣为原料,对其中所含的砷进行回收。分别考察了碱用量、浸出温度、液固比和浸出时间对砷浸出率的影响及溶液初始pH、钙砷摩尔比和沉淀时间对砷沉淀率的影响。通过单因素条件试验确定了浸砷的较优条件为:氢氧化钠浓度为240 g/L,反应温度60 ℃,液固比4∶1,搅拌浸出2 h。在最优条件下砷浸出率达到85%。从浸出液中沉砷的较优条件为:溶液初始pH=12.0,钙砷摩尔比2∶1,沉淀时间30 min。在优化条件下砷沉淀率达到97%以上。
中文关键词: 含砷矿渣  氢氧化钠  浸出  砷
Abstract:With bio-oxidation gold ore slag as the raw material, arsenic was recycled from the slag. In the arsenic leaching test, four factors had been studied including the usage of sodium hydroxide, leaching temperature, the ratio of liquid to solid(L/S), and leaching time. In the arsenic precipitate test, three factors including the initial solution pH, the mole ratio between Ca and As and the reaction time had been studied. The optimum conditions for arsenic leaching include the optimal amount of NaOH of 240g/L, 60 ℃, L/S= 4/1, 2 h. Under the optimum conditions, the leaching rate of arsenic was 85%. The optimum conditions for arsenic precipitating include the initial solution pH of 12.0 and the mole ratio between Ca and As of 2∶1, 30 min, under which more than 97% of arsenic would be precipitated.
文章编号:     中图分类号:    文献标志码:
基金项目:
引用文本:
孙光勇 王卫亭 杨军 杨譞 张永奎.含砷金矿提金渣综合回收砷[J].有色金属(冶炼部分),2011(12):11-14.
SUN Guang-yong, WANG Wei-ting, YANG Jun, YANG Xuan, ZHANG Yong-kui.Comprehensive Recovery of Arsenic from Gold Ore Slag[J].Nonferrous Metals (Extractive Metallurgy),2011(12):11-14.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号