氧压浸出处理低铁闪锌矿
(东北大学 材料与冶金学院,多金属共生矿生态化利用教育部重点试验室)
Oxygen Pressure Leaching on Low Iron Sphalerite
(Key Laboratory of Ecological Utilization of Multi-metal Intergrown Ores of Ministry of Education, School of Materials and Metallurgy, Northeastern University)
摘要
图/表
参考文献
相似文献
本文已被:浏览 3801次   下载 63次
投稿时间:2011-05-23               
中文摘要: 以低铁闪锌矿精矿为原料,采用氧压浸出技术进行处理。绘制了150 ℃、1.0 MPa的ZnS-H2O系电位-pH图。通过单因素试验确定各因素的影响趋势,采用ICP、XRD、XRF和BET等检测方法对浸出液和浸出渣进行分析表征,确定最佳浸出条件为:精矿粒度-0.075 mm~+0.055 mm、浸出温度150 ℃、氧分压0.8 MPa、初酸浓度15%、浸出时间90 min、浸出液固比6∶1~8∶1、搅拌转速500 r/min、添加剂用量1.0%。在此条件下,锌浸出率在97%以上,硫转化率达到90%,实现了精矿中锌的充分浸出与渣中元素硫的富集。
Abstract:Oxygen pressure leaching process was applied to treat low iron sphalerite concentrate. Eh-pH diagram of ZnS-H2O system at 150 ℃ and 1.0 MPa was drew. The single factor experiments were performed in autoclave, the leachate and residue were characterized by ICP, XRD, XRF and BET. The results indicate when particle size is -0.075 mm~+0.055 mm, temperature is 150 ℃, oxygen partial pressure is 0.8 MPa, initial acid concentration is 15%, leaching time is 90 min, leaching liquid-solid ratio is 6∶1~8∶1, stirring speed is 500 r/min, and additive amount is 1.0%, extraction rate of zinc is above 97% and conversion rate of sulfur is about 90%. Sufficiently leaching of zinc and enriching of element sulfur in the residue were achieved via the process.
文章编号:     中图分类号:    文献标志码:
基金项目:国家自然科学基金资助项目(51004033, 50974035, 51074047);国家“十一五”科技支撑计划项目(2008BAB34B01);教育部高校博士点专项基金项目(20050145029);辽宁省优秀青年科技人才基金项目(2005221012)
引用文本:
古岩,张廷安,吕国志,牟望重,豆志河.氧压浸出处理低铁闪锌矿[J].有色金属(冶炼部分),2011(10):1-5.
GU Yan,ZHANG Ting-an,LV Guo-an,MOU Wang-zhong,DOU Zhi-he.Oxygen Pressure Leaching on Low Iron Sphalerite[J].Nonferrous Metals (Extractive Metallurgy),2011(10):1-5.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号