中文摘要: 以铜阳极泥渣为原料,探讨了碲的浸出条件。通过正交试验与单因素试验考察了浸出时间、温度、pH及高锰酸钾加入量对碲浸出率的影响。结果表明,最佳浸出工艺条件为:浸出时间4 h、浸出温度70 ℃、高锰酸钾用量0.8%、pH 1.6左右。在最佳浸出条件下,碲浸出率达92.15%。
Abstract:The extraction conditions of tellurium were discussed using tellurium-bearing residue from copper anode slime as raw materials. The effect of leaching time, temperature, dosage of potassium permanganate and pH on tellurium extracting rate were investigated through orthogonal experiment and factor experiment. The results show that the optimum leaching condition is that leaching time of 4 h, temperature of 70 ℃, the dosage of potassium permanganate of 0.8%, pH=1.6. Under above conditions, the tellurium leaching rate was 92.15%.
文章编号: 中图分类号: 文献标志码:
基金项目:
引用文本:
康立武,闵昌松,彭樟成.铜阳极泥渣中浸出碲的试验研究[J].有色金属(冶炼部分),2011(6):3-5.
KANG Li-wu,MIN Chang-song,PENG Zhang-cheng.Experimental Study on Leaching of Tellurium from Residue of Copper Anode Slime[J].Nonferrous Metals (Extractive Metallurgy),2011(6):3-5.
康立武,闵昌松,彭樟成.铜阳极泥渣中浸出碲的试验研究[J].有色金属(冶炼部分),2011(6):3-5.
KANG Li-wu,MIN Chang-song,PENG Zhang-cheng.Experimental Study on Leaching of Tellurium from Residue of Copper Anode Slime[J].Nonferrous Metals (Extractive Metallurgy),2011(6):3-5.

关注微信公众号