中文摘要: 以澳大利亚某红土镍矿为原料,采用两段硫酸化焙烧—水浸工艺回收镍钴。重点探讨酸料比、低温焙烧段温度及时间、高温焙烧段温度及时间对镍钴浸出率的影响。结果表明,在酸料比为0.6,一段低温焙烧温度250 ℃,焙烧时间60 min,二段高温焙烧温度650 ℃,焙烧时间3 h的条件下进行硫酸化焙烧,焙烧产物经过水浸,Ni和Co浸出率分别达到93.38%和91.95%。
中文关键词: 红土镍矿  硫酸化焙烧  水浸  镍  钴
Abstract:Ni and Co was recovered from an Australia nonferrous nickel laterite by two stages sulpation roasting-water leaching process. The process and conditions was studied. The effects of acid to materials ratio, roasting temperature and time in low roasting action and high roasting action on Ni and Co leaching rate were investigated, respectively. The results show that the sulfation roasting is performed under the conditions of sulfuric acid to materials ratio 0.6, first low temperature roasting temperature 250 ℃, roasting time 60 min, second high temperature roasting temperature 650 ℃, roasting time 3 h; the roasted product is subjected to water leaching, the leaching rate of Ni and Co are up to 93.38% and 91.95%, respectively.
文章编号:     中图分类号:    文献标志码:
基金项目:国家科研院所技术开发专项资金(NCSTE-2007-JKZX-062),云南省科技计划项目(2008AA001)
引用文本:
汪云华,董海刚,范兴祥,吴跃东,赵家春,暂林寒,李柏榆,李楠.两段硫酸化焙烧-水浸从红土镍矿中回收镍钴[J].有色金属(冶炼部分),2012(2):16-18.
Wang yunhua,Dong haigang,Fan xingxiang,Wu yuedong,Zhao jiachun,Zan linhan,Li baiyu,Li nan.Recovery of Ni and Co from Nickel Laterite with Two Stages Sulphation Roasting—Water Leaching Process[J].Nonferrous Metals (Extractive Metallurgy),2012(2):16-18.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号