本文已被:浏览 2944次 下载 27次
中文摘要: 对不同粒度(-10 mm、-8 mm、-6 mm)的矿石进行了柱浸试验,考察了筑堆粒度对浸出率、浸出周期及耗酸等的影响,试验结果表明适应与该矿点堆浸工艺的最佳筑堆粒度为-8 mm。
Abstract:The different particle size of heap leaching experimentation is expatiated,the inflence of particle size on leaching efficency,leaching cycle and expend acid were studied,the results show that the optimum particle size is 8 mm for heap leaching.
keywords: Uranium Heap leaching Particle size
文章编号: 中图分类号:TD92 文献标志码:
基金项目:
陈家富
东华理工大学;
陈家富' target='_blank'>CHEN Jia-fu
East China Institute of Technology/a>;Fuzhou 344000/a>;China
引用文本:
陈家富.不同粒度柱浸浸铀试验研究[J].有色金属(冶炼部分),2010(1):.
.Study on Different Particle Size of Uranium Ore Leaching[J].Nonferrous Metals (Extractive Metallurgy),2010(1):.
陈家富.不同粒度柱浸浸铀试验研究[J].有色金属(冶炼部分),2010(1):.
.Study on Different Particle Size of Uranium Ore Leaching[J].Nonferrous Metals (Extractive Metallurgy),2010(1):.