本文已被:浏览 2650次 下载 25次
中文摘要: 石煤中加入石灰和适量的添加剂焙烧,焙砂用NH4HCO3和NaHCO3溶液浸出,浸出液经离子交换树脂吸附,可制得纯度达到国标99级以上的V2O5。在焙烧过程中解决了传统钠化焙烧的废气污染问题,经交换吸附后的废水可直接回用于浸出,不影响浸出率和产品质量。
Abstract:CaO and some additives was added to the stone coal when it was roasted and then the calcine was leached in NH4HCO3 and NaHCO3 solution.The V2O5 which purity is above 99% was got from the ion-exchange absorb process of the leached solution.Compared with conventional roasting-sodium oxidization method,this method solved the pollution of the waste gas and wastewater.the wastewater discharged from the absorb process can be directly reused into the leaching process without any effect on the leaching rate and qua...
文章编号: 中图分类号:TF841.3 文献标志码:
基金项目:
DAI Wen-can SUN Shui-yu
Department of Environmental Engineering/a>;Guangdong University of Technology/a>;Guangzhou 510006/a>;China
引用文本:
戴文灿,孙水裕.清洁型石煤提钒新工艺[J].有色金属(冶炼部分),2010(1):.
.Study on the New Clean Technology of Vanadium Extraction from Stone Coal[J].Nonferrous Metals (Extractive Metallurgy),2010(1):.
戴文灿,孙水裕.清洁型石煤提钒新工艺[J].有色金属(冶炼部分),2010(1):.
.Study on the New Clean Technology of Vanadium Extraction from Stone Coal[J].Nonferrous Metals (Extractive Metallurgy),2010(1):.