中文摘要: 某地蛇纹石矿中镍主要以类质同象存在于硅酸盐矿物内,且粒度很细,不能用物理方法予以富集。为此,采用硫酸浸出工艺,镍浸出率为85.7%浸出贵液经净化沉镍,可得含镍41.24%的Ni(OH)2镍精矿,沉镍收率88.6%,综合收率达75.93%。
Abstract:Ni mainly exists in silicate as an isomorphous element in serpentine,and silicate is fine dissemination particle,that couldn't concentration with physical method.Acid leaching technology was adopted to treat this ore,the results show that leaching rate of Ni was 85.7%,and Ni(OH)_2 concentration containing 41.24% Ni from the noble solution after purifying and precipitating,the precipitating rate of Ni was 88.6% and the total recovery rate of Ni was 75.93%.
keywords: Nickel,Acid leaching process,Serpentine,
文章编号: 中图分类号:TF815 文献标志码:
基金项目:
引用文本:
罗仙平,龚恩民.酸浸法从含镍蛇纹石中提取镍的研究[J].有色金属(冶炼部分),2006(4):28-31.
.Experimental Study on Nickel Extraction from Serpentine with Acid Leaching Technology[J].Nonferrous Metals (Extractive Metallurgy),2006(4):28-31.
罗仙平,龚恩民.酸浸法从含镍蛇纹石中提取镍的研究[J].有色金属(冶炼部分),2006(4):28-31.
.Experimental Study on Nickel Extraction from Serpentine with Acid Leaching Technology[J].Nonferrous Metals (Extractive Metallurgy),2006(4):28-31.

关注微信公众号