本文已被:浏览 2223次 下载 18次
中文摘要: 闪速炉处理铅、锌、砷等杂质含量较高的精矿时出现了炉况较大的波动,沉淀池粘渣厚;沉淀池侧壁、上升烟道喉口部及侧壁、废热锅炉入口等处出现结瘤;冲渣水沟堵塞漫水等一系列问题。对出现此类问题的原因进行了分析,采取了相应的防范措施,得到了预期的效果。
Abstract:When smelting concentrate containing high impurities such as Pb, Zn, As, flash furnace suffered fluctuation in furnace condition, thick sticky slag layer in settler, accretion formation on settler wall, uptake throat and boiler entrance. Additionally, the groove of granulation circulation water is easy to be built up with water flooding. This paper analyzes factors causing the above troubles, and presents the corresponding precautions to them as well as the results expected.
文章编号: 中图分类号:TF811 文献标志码:
基金项目:
昂正同
金隆铜业有限公司,安徽铜陵244021
昂正同' target='_blank'>ANG Zheng-tong
引用文本:
昂正同.闪速炉处理高Pb、Zn、As精矿的探讨[J].有色金属(冶炼部分),2005(1):32-35.
.Inquisition on Smelting High Pb, Zn, As Concentrate in Flash Furnace[J].Nonferrous Metals (Extractive Metallurgy),2005(1):32-35.
昂正同.闪速炉处理高Pb、Zn、As精矿的探讨[J].有色金属(冶炼部分),2005(1):32-35.
.Inquisition on Smelting High Pb, Zn, As Concentrate in Flash Furnace[J].Nonferrous Metals (Extractive Metallurgy),2005(1):32-35.