本文已被:浏览 3137次 下载 25次
投稿时间:2011-02-01
投稿时间:2011-02-01
中文摘要: 通过合理控制冷摆碾成形工艺参数,成功制备出形状尺寸满足要求、表面质量良好的钽合金薄壁回转体零件,研究了冷变形后钽合金的再结晶退火工艺,检测了退火后钽合金零件的力学性能和硬度分布,观察了径向不同位置的显微组织。结果表明,经过1 350 ℃×60 min真空退火,钽合金发生了完全再结晶,平均晶粒尺寸50 μm左右,零件不同位置的组织均匀性较好,抗拉强度达到360 MPa,延伸率45.5%。
Abstract:Tantalum alloy thin-walled rotating part with qualified size and good surface quality could be obtained through the reasonable control of rotary forging processing parameters. The recrystallization annealing process of cold-forming tantalum alloy was studied, the mechanical property and hardness distribution was checked, the microstructure of the part annealed was observed. The results show that tantalum alloy part annealed by 1 350 ℃×60 min is fully recrystallized, the average grain size is about 50μm;The tantalum alloy part possesses good uniformity microstructure, and tensile strength is 360 MPa, elongation rate is 45.5%.
文章编号: 中图分类号: 文献标志码:
基金项目:
| 作者 | 单位 |
| 李祥 | 北京有色金属研究总院有色金属加工工程研究中心 |
| 李彦利 | 北京有色金属研究总院有色金属加工工程研究中心 |
| 李德富 | 北京有色金属研究总院有色金属加工工程研究中心 |
| 闫晓东 | 北京有色金属研究总院有色金属加工工程研究中心 |
| 彭海健 | 北京有色金属研究总院有色金属加工工程研究中心 |
引用文本:
李祥,李彦利,李德富,闫晓东,彭海健.钽合金零件冷摆碾成形组织性能研究[J].有色金属(冶炼部分),2011(5):52-55.
LI Xiang,LI Yan-li,LI De-fu,YAN Xiao-dong,PENG Hai-jian.Microstructure and Mechanical Properties of Ta-W Alloy Part Formed by Cold Rotary Forging[J].Nonferrous Metals (Extractive Metallurgy),2011(5):52-55.
李祥,李彦利,李德富,闫晓东,彭海健.钽合金零件冷摆碾成形组织性能研究[J].有色金属(冶炼部分),2011(5):52-55.
LI Xiang,LI Yan-li,LI De-fu,YAN Xiao-dong,PENG Hai-jian.Microstructure and Mechanical Properties of Ta-W Alloy Part Formed by Cold Rotary Forging[J].Nonferrous Metals (Extractive Metallurgy),2011(5):52-55.