中文摘要: 采用高温氯化工艺对新疆某提金渣进行提取金、银等有价元素的研究。结果表明:在干式混料,粉状焙烧,氯化挥发温度1 000 ℃,氯化时间30 min,CaCl2用量5%的条件下,金、银挥发率分别为95.19%和59.26%。
Abstract:Study on extraction of gold and silver from gold-extraction residue with the process of high temperature chloridization was conducted. The results indicate that the volatilization rate of gold and silver is 95.19% and 59.26%, respectively, under the conditions including adopt dry type mixing and powdered roasting, chloridization volatilization temperature of 1 000 ℃, chloridization time of 30 min, and the consumption of CaCl2 of 5%.
文章编号: 中图分类号: 文献标志码:
基金项目:
引用文本:
黄海辉,王云,袁朝新,李云.从提金渣中回收金银的研究[J].有色金属(冶炼部分),2011(10):37-39.
HUANG Hai-hui,WANG Yun,YUAN Chao-xin,LI Yun.Extraction of Gold and Silver from Gold-extraction Residue[J].Nonferrous Metals (Extractive Metallurgy),2011(10):37-39.
黄海辉,王云,袁朝新,李云.从提金渣中回收金银的研究[J].有色金属(冶炼部分),2011(10):37-39.
HUANG Hai-hui,WANG Yun,YUAN Chao-xin,LI Yun.Extraction of Gold and Silver from Gold-extraction Residue[J].Nonferrous Metals (Extractive Metallurgy),2011(10):37-39.