低品位氧化钼精矿高压浸出新工艺研究
(中国地质科学院郑州矿产综合利用研究所)
Rresearch on Molybdenum Extraction from Oxidation Molybdenum Concentrates
(Zhengzhou Institute of Multipurpose Utilization of Mineral Resources, CAGS, National Research Center of Multipurpose Utilization of Non-metallic Mineral Resources)
摘要
图/表
参考文献
相似文献
本文已被:浏览 3238次   下载 55次
投稿时间:2010-06-11               
中文摘要: 针对某氧化钼精矿钼含量低、脉石矿物方解石含量高的特点,采用碳酸钠溶液高压浸出新工艺处理该原料,最佳浸出条件为:碳酸钠用量为理论量1倍、浸出时间1 h、浸出温度160 ℃、液固比1.5。最佳浸出条件下,钼浸出率大于97%。
Abstract:According to the characters that low content of molybdenum and high content of calcspar in the oxidation molybdenum concentrates, the high pressure leaching process was adopted. In the leaching process sodium carbonate was used as leaching regent. The results showed that the optimal quantity of sodium carbonate was 1 times of its theoretical quantity, the optimal leaching time was 1 h, the optimal leaching temperature was 160 ℃ and the liquid-solid ratio was 1.5. The leaching rate was more than 97% under the optimal leaching condition.
文章编号:     中图分类号:    文献标志码:
基金项目:
引用文本:
曹耀华,刘红召,高照国,杨绍文.低品位氧化钼精矿高压浸出新工艺研究[J].有色金属(冶炼部分),2011(1):5-8.
CAO Yao-Hua,LIU Hong-zhao,GAO Zhao-guo,YANG Shao-wen.Rresearch on Molybdenum Extraction from Oxidation Molybdenum Concentrates[J].Nonferrous Metals (Extractive Metallurgy),2011(1):5-8.

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
86-10-63299752/63299758

联系我们

电话:010-63299752/63299758

传真:010-63299744

QQ:XXXXXXX

Email:ysyl@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地18区23号楼

关注微信公众号