中文摘要: 采用实际生产电解槽的1:1 000规模,控制阴极电流密度450 A/m2,电积液温度37~40 ℃,电积液中的Zn2+浓度53~58 g/L,硫酸浓度170~180 g/L,连续电积48 h,研究了骨胶对长周期锌电积的直流电单耗、电流效率和阴极锌表面质量的影响。结果表明,吨锌骨胶加入量控制在0.1~0.3 kg,可以使48 h锌电积的槽电压保持在2.99~3.05 V,吨锌直流电单耗在2 820~2 860 kw?h,而电流效率均高于90%,所产阴极锌表面光滑致密;吨锌骨胶加入量超过0.3 kg将使锌电积的直流电单耗显著升高、电流效率明显降低,且所产阴极锌表面粗糙、生长大量突瘤、颜色暗沉。
Abstract:the effects of glue on power consumption, current efficiency and physical characteristics of zinc deposits of long period zinc electrodeposition from acidic sulfate electrolyte were investigated. The volume of the electrolyzer used in the test was of one thousandth of the electrolyzer used in workshop. The electrowinning experiments were ongoing for 48 hours, keeping current density of 450 A/m2, the temperature of electrolyte at 37~39 ℃, the concentration of Zn2+ at 53~58 g/L, the concentration of H2SO4 at 170~180 g/L. The results show that the per ton zinc dosages of glue of 0.1~0.3 kg will lead to cell voltage of 2.99~3.05 V, per ton zinc power consumption of 2 820~2 860 kw?h and current efficiency of more than 90%. The deposits morphology of zinc were smooth and compact. The per ton zinc dosages of glue of more than 0.3 kg will cause significant increase in power consumption, and decrease in current efficiency. The deposits morphology of zinc were rough, dull and with much dendrites.
文章编号: 中图分类号: 文献标志码:
基金项目:
引用文本:
黄娟,李坚,孙成余,罗永光,施哲.骨胶对长周期锌电积能耗及阴极质量的影响[J].有色金属(冶炼部分),2011(1):12-15.
HUANG Juan,LI Jian,SUN Cheng-yu,LUO Yong-guang,SHI Zhe.Effects of Glue on Power Consumption and Quality of Cathode Zinc of the Long Period Zinc Electrodeposition[J].Nonferrous Metals (Extractive Metallurgy),2011(1):12-15.
黄娟,李坚,孙成余,罗永光,施哲.骨胶对长周期锌电积能耗及阴极质量的影响[J].有色金属(冶炼部分),2011(1):12-15.
HUANG Juan,LI Jian,SUN Cheng-yu,LUO Yong-guang,SHI Zhe.Effects of Glue on Power Consumption and Quality of Cathode Zinc of the Long Period Zinc Electrodeposition[J].Nonferrous Metals (Extractive Metallurgy),2011(1):12-15.

关注微信公众号